设计师 Xiangzhi Zhao 的作品 Morning Dew 再生戒指 荣获了极具声望的 2020 A' Design Award 铜奖,竞赛类别为珠宝设计。
铜珠宝· 2020
Morning Dew 再生戒指
设计师: Xiangzhi Zhao
客户: Dist industrial design studio
珠宝类别A' Design Award 铜奖获奖者
已验证的获奖者
验证 #103005 的获奖状态设计作品
关于 Morning Dew 再生戒指
“晨露”这款首饰在设计时重点关注了材料,利用更加绿色的回收贵金属手段制取再生金银为材料,围绕着这种材料设计了一个以藤蔓包裹露水形态为灵感的戒指。一块报废的电路板比起一块同质量的金矿而言含金量前者高于后者太多,因此对于电子废弃物的环保再利用是一座人们涉足很少的金山。希望“晨露”的设计为减少资源浪费,提倡资源回收的大趋势中提供一项方法指引。
荣誉认可
关于A' Design Award 铜奖
Morning Dew 再生戒指是 A' Design Award 铜奖得主,这是授予以创造力、独创性和敏锐见长的杰出设计的极具声望的认可。铜奖得主是技艺娴熟、创意惊人的作品,印证了其设计师丰富的经验、想象力与机智。预计Morning Dew 再生戒指将成为一件备受推崇、令人钦佩且被珍爱的物品,兼具显著的专业性与创新性。这件赢得 A' Design Award 铜奖的设计融入艺术、科学、设计和技术领域的最佳实践,并因注重细节而出类拔萃。Morning Dew 再生戒指出色地满足需求,触动渴望,迷住情感,并吸引好奇心。
设计幕后
媒体资料包
由设计师提供的致谢、团队成员及技术详情。
- 独特属性
- The ring was designed with a focus on materials. In designing the "morning dew", an original and greener method of recovering precious metals is used to prepare regenerated gold and silver as materials. The preparation method is simply to use an amine-containing porous material to adsorb selected metal ions, and to achieve reuse of the treatment liquid in the treatment process, so as to recover precious metals by more environmentally friendly methods.
- 尺寸与包装
- Width 20 mm x Depth 20 mm x Height 4 mm
- 标签
- Ring, Grace, environmental protection, New material, Artistic
- 生产技术
- The original green precious metal recovery method is to copolymerize 4,4 '- (hexachloroisopropyl) bisphenol with melamine in alkaline solution, the obtained amine-containing porous material can absorb selected metal ions in the solution, and the treatment liquid can be reused to reduce the production of waste water. The material used in “morning dew " is made entirely from this extraction method.
- 设计挑战
- The molar ratio of cyanamide to hexachlorophenol A is from 3:1.9 to 3: 2.2. Whenthe molar ratio is less than 3:1.9 or more than 3:2.2, the yield is significantly reduced. This characteristic is obtained through numerous experiments. In order to design a metal method with more high-yield regeneration, much efforts and experiments must be made.
- 研究
- Through many experiments and comparative analysis, it is concluded that the dehydration reaction temperature of the material used for regenerating metal is 136-140 celsius degree, the reaction time is 3-5 hours, and when the time is less than 3 hours, the polycondensation is incomplete and the yield is low.
- 灵感
- According to UNEP, an average of 1 ton of ordinary electronic waste contains 490 kg of metal. If not recycled, it will cause a huge waste of resources. The most commonly used pyrometallurgical technology for disposal of electronic waste will produce toxic gases, such as fluorocarbons, bromine flame retardants and organic compounds, which tend to generate dioxins under oxidation conditions. In recent years, the solid-phase extraction method has less solvent consumption, simple reaction and fast speed. However, waste of liquid of this technology has become a problem in treatment process.
- 项目周期
- The project began in Beijing in 2018, applied for a technology patent in early 2019, and was completed in 2019.
- 操作流程
- The design of “morning dew " ring focuses on the material, which is made of regenerated gold and silver by a greener way of recovering precious metals. Based on this material, a ring with the shape of dew, wrapped by vines, is designed. A scrap circuit board is much more valuable than a gold mine of the same quality in terms of gold proportion. Therefore, reuse of electronic waste is not receiving enough attention but worth of attention and implementation. It is hoped that the design of "morning dew" will provide guidance of reducing resource waste and promoting resource recovery.